熱風爐用低蠕變高鋁磚
項目 \ 指標 \ 牌號 | 高鋁磚 | 低蠕變高鋁磚 | |||
RL-65 | RL-55 | RL-48 | RDLZ-75 | RDLZ-65 | |
AL2O3 % | ≥65 | ≥55 | ≥48 | ≥75 | ≥65 |
體積密度g/cm3 BD | ≥2.75 | ≥2.70 | |||
顯氣孔率% AP | ≤24 | ≤24 | ≤24 | ≤18 | ≤19 |
常溫耐壓強度MPa CCS | ≥50 | ≥44.5 | ≥39.8 | ≥80 | ≥80 |
耐火度℃ | ≥1790 | ≥1790 | ≥1750 | >1790 | >1790 |
荷重軟化溫度℃RUL | ≥1500 | ≥1470 | ≥1420 | ≥1620 | ≥1590 |
重燒線變化1500℃×2h% | +0.0 -0.4 | +0.0 -0.4 | (1450℃×2h)+0.0-0.4 | 0.2 | 0.4 |
蠕變率% | (1450℃×50h)-0.50 | (1450℃×50h)-0.80 |